How does Atomic Layer Deposition differ from Chemical Vapor Deposition?

While both ALD and CVD are used for thin film deposition, ALD provides more precise control over the thickness and composition of the film. This precision is achieved through the sequential exposure of the substrate to different precursors, allowing for the deposition of ultrathin layers.