The mechanism behind negative resists involves the cross-linking of polymer chains upon exposure to radiation. This cross-linking increases the molecular weight and decreases the solubility of the material in the developer solution. Consequently, the exposed areas remain intact while the unexposed areas are dissolved away. This is in contrast to positive resists, where the exposed areas become soluble and are removed during development.